BUBBLE FORMATION FROM NON-WETTED ORIFICES UNDER CONSTANT FLOW RATE
GAO Qin DONG Liang CHENG Lanzheng GAO Hongwu GUO Keren (Dalian Institute of Technology)
Cite this article: 

GAO Qin DONG Liang CHENG Lanzheng GAO Hongwu GUO Keren (Dalian Institute of Technology). BUBBLE FORMATION FROM NON-WETTED ORIFICES UNDER CONSTANT FLOW RATE. Acta Metall Sin, 1987, 23(1): 138-140.

Download:  PDF(256KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made on the bubble formation from non-wetted orifices in water and in molten Al under condition of constant flow rate.The effects of the geometric parameters of orifice hole and surface roughness of orifices upon the size of bubble have also been exa- mined.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/138

1 Pritz W.Phys Z,1935;36:379
2 Mori K,Ozawa Y.Sano.M.Trans Iron Steel Inst Jpn,1982;22:377
3 Wraith A E.Chem Eng Sci,1971;26:1659
No related articles found!
No Suggested Reading articles found!