NOTE ON THE Fe-Pb PHASE DIAGRAM
XING Zhong shu (Institute of Metal Research.Academia Sinica;Shenyang)
Cite this article: 

XING Zhong shu (Institute of Metal Research.Academia Sinica;Shenyang). NOTE ON THE Fe-Pb PHASE DIAGRAM. Acta Metall Sin, 1987, 23(1): 115-119.

Download:  PDF(374KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To elucidate the relation between optimum solubility and temperature,the critical assessment of the experimental data of solubility of Pb in liquid Fe,or of Fe in liquid Pb,have been made.By combining these relations with the liquids curve calculated from Clausius-Clapeyron equation,the composition and temperature of the monotectic point on the Fe-Pb phase diagram have been esti- mated.Thus,an Fe-Pb phase diagram may be drawn on the basis of above men- tioned studies.
Received:  18 January 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I1/115

1 Kubaschewski O,Iron-Binary Phase Diagrams,Springer-Verla.1982;87-88
2 Stevenson D A,Wulff J.Trans Metal1 Soc AIME,1961;221:271
3 Miller K O,Elliott J F,Trans Metal1 Soc AIME 1960;218:900
4 Morozov A N,Ageyev Yu A.Russ Metall,1971;4:78
5 Lord A E,Parlee N A.Trans Metall Soc AIME,1960;218:644
6 Araki T,Trans Natl Res Inst Met(Tokyo),1963;5:91
7 荒木透,小柳明,大场健二,大桥久道.铁と钢,1963;49:421
8 Kubaschewski O,High Temp High Pressures,1981;13:435
9 Kubaschewski O,Alcock C B.Metallurgical Thermochemistry,5th ed,Pergamon Press.1979
No related articles found!
No Suggested Reading articles found!