| CREEP BEHAVIOR OF METALLIC GLASSES——AN EXPERIMENTAL STUDY |
| MA Xueming HE Yizhen (Institute of Solid State Physics.Academia Sinica.Hefei) |
|
Cite this article:
MA Xueming HE Yizhen (Institute of Solid State Physics.Academia Sinica.Hefei). CREEP BEHAVIOR OF METALLIC GLASSES——AN EXPERIMENTAL STUDY. Acta Metall Sin, 1987, 23(1): 120-125.
|
|
|
Abstract This work is a systematic study of the creep behavior of metallic glasses, α-Pd_(80)Si_(20) and Cu_(60)Zr_(40).In particular,we studied the influence of stress,temper- ature and pre-annealing treatments on creep curves.Quantitative relations be- tween viscosity and the pro-annealing parameters(t_a and T_a)were obtained as following: η=K_1+K_2 ln t_a and η=C exp(T_a/α) Results were also obtained for“Changing-Load Creep”and“Secon-drun Creep” measurements.
|
|
Received: 18 January 1987
|
1 Perez J,Fouqnet F.He Y(何怡贞).Phys Status Solidi(a),1982;72:289 2 Taub A I,Spaepen F.Acta Metall,1980;28:1781 3 Spaepen F.Acta Metall,1977;25:407 4 Taub A I,Spaepen F.Sct Metall,1980;14:1197 5 Mulder A L,Derksen R J.Prijver J W.et al,J Phys(Paris).Colloq.C8. 1980;41:843 6 Taub A I,Luborsky F E.Acta Metall,1981;29:1939 7 Argon A S,Kuo H Y.J Non-Cryst Solids,1980;37:241 8 Patterson J P,Jones D R H.Acta Metall,1980;28:675 9 Egami T,J Mater Sci,1978;13:2587 10 Luborsky F E.Walter J L.General Electric Research Development Laboratory Reports 78CR D063. New York:Schenectady,1978.( |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|