Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (6): 103-109    DOI:
Current Issue | Archive | Adv Search |
OPTIMIZING MODEL OF ENERGY UTILIZATION FOR IRONMAKING SYSTEM OF A STEEL WORKS
by MA Hongyi; LU Zhongwu (Northeast Institute of Technology; Shenyang)
Cite this article: 

by MA Hongyi; LU Zhongwu (Northeast Institute of Technology; Shenyang). OPTIMIZING MODEL OF ENERGY UTILIZATION FOR IRONMAKING SYSTEM OF A STEEL WORKS. Acta Metall Sin, 1986, 22(6): 103-109.

Download:  PDF(496KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Taking a steel works as an example, the factors which influence overall energy consumption of the ironmaking system and their dependences were discussed with view of comprehensive energy conservation, the optimizing model of ironmaking system for energy utilization was developed. The model consists of two parts, the general model of ironmaking system and submodel of sintering process, both are nonlinear program model. The optimum charge mixture in sintering process and optimum ratio of sinter and pellet were researched by the model and optimization method, the influence of the parameters of processes on the overall energy consumption of ironmaking system was also dealt with.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/103

沈昌炽;任暁茹,冶金能源,2(1983) ,№2,10.
2 Gray, W.R.; Fekete, J.D.; Tarkoff, M. I., Iron Steel Eng., 51 (1974) , № 11, 54.
3 松永研一郎,熟管理と公害,28(1976) ,№ 1,29.
4 陆钟武;周大刚,钢铁,16(1981) .№ 10. 63.
5 Himmelblau. D. M., 张义等译,实用非线性规划,科学出版社,1981,p.376.
6 马弘毅,东北工学院硕士论文,1984.
No related articles found!