Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 78-84    DOI:
Current Issue | Archive | Adv Search |
DISTRIBUTION OF Al AND Ce BETWEEN Ag AND Fe
ZHOU Jicheng (Shanghai Institute of Metallurgy; Academia Sinica); TIAN Yahwen; MA Yonghui; ZHU Limin (North-East Institute of Technology; Shenyang);
Cite this article: 

ZHOU Jicheng (Shanghai Institute of Metallurgy; Academia Sinica); TIAN Yahwen; MA Yonghui; ZHU Limin (North-East Institute of Technology; Shenyang);. DISTRIBUTION OF Al AND Ce BETWEEN Ag AND Fe. Acta Metall Sin, 1986, 22(5): 78-84.

Download:  PDF(489KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  For the purpose of studying the influence of Ca on the activity coefficient of Al, f_(Al)~(Ca), in Ag, the dependence of the distribution ratio R_(Al)(=[%Al]_(Fe)/[%Al]_(Ag)) on Ca content in Ag was determined at 1600℃. The results obtained can be expressed as follows: R_(Al)=-2.91(%Ca)~2+3.51(%Ca)+3.05 and the interaction coefficient can be evaluated as lgf_(Al)~(Ca)=-0.441(%Ca)~2+0.476(%Ca) with Ca content within the range of 0 to 0.54%. The interaction parameters e_(Al)~(Ca) and e_(Ca)~(Al) are evaluated as 0.476 and 0.705 respectively. Preliminary results obtained on the distribution of Ce between Ag and Fe show that R_(Ce)(=[%Ce]_(Fe)/[%Ce]_(Ag)) is as low as 3.70×10~(-3). Besides, some thermodynamic functions are also deduced from the experimental results mentioned above.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/78

1 Chipman, J., Trans. ASM. 22 (1934) , 385.
2 Chou, Y.H., Doctorate Thesis, Department of Metallurgy, Carneige Institute of Technology. 1947.
3 王渭源,邹元燨,科学通报,(1957) ,№ 9. 287.
4 Schenck, H.; Neuman, F., Arch. Eisenhuettenws., 29 (1958) , 263.
5 黄磊;邹元燨,研究生论文,中国科学院上海冶金研究所,1965.
6 邹元燨;周继程等,某种稀土合金制备的研究,未公开发表资料,1959.
7 王常珍;邹元燨,金属学报,16(1980) ,191.
8 洪彦若,白江添,金属学报,15(1979) ,51.
9 Cafasso, F.A.; Feder, H.M.; Johnson, I., J. Phys. Chem., 68 (1964) , 1944.
10 #12
11 Lupis, C.H.P.; Elliott, J.F., Trans. Metall. Soc. AIME, 223 (1965) , 257.
12 邹元燨;伊立奥特,化学学报,22(1956) ,№ 1,14.
13 Kubaschewski, O.; Alcock, C.B., Metallurgical Thermochemistry, 5th, ed., Oxford Pergamon, 1979.
14 Gaskell, D.R., Introduction to Metallurgical Thermodynamics, 2nd ed., McGraw-Hill, New York, 1981.
15 Gokcen, N.A.; Chipman, J., Trans. AIME, 197 (1953) . 173.
No related articles found!
No Suggested Reading articles found!