A NEW POLYMERIZATION MODEL APPLYING TO LIQUID SILICATE SYSTEM CaO-SiO_2
WANG Zhichang (Shanghai Institute of Nuclear Research; Academia Sinica); ZHOU Jicheng; CHENG Zhaonian (Shanghai Institute of Metallurgy; Academia Sinica)
Cite this article: 

WANG Zhichang (Shanghai Institute of Nuclear Research; Academia Sinica); ZHOU Jicheng; CHENG Zhaonian (Shanghai Institute of Metallurgy; Academia Sinica). A NEW POLYMERIZATION MODEL APPLYING TO LIQUID SILICATE SYSTEM CaO-SiO_2. Acta Metall Sin, 1986, 22(5): 69-77.

Download:  PDF(642KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The use of the s-regular anion sub-lattice assumption instead of the ideal anion sub-lattice one in the Whiteway, Smith and Masson (WSM) model leads to a four-parameter branched chain polymerization model for the binary silicate melts. For most slags investigated so far, three interchange energy parameters in the present model, W_(12), W_(o1) and C (C=W_(o2)-W_(o1)), could be assumed to be zero; then it becomes an one-parameter model, i.e. the WSM model. For the CaO-SiO_2 melts, the three above-mentioned parameters could be assumed to have the same value that does not equal zero. The new model is then converted into a twoparameter model. With the interchange energy parameter W_(12)/RT=-0.023 and the thermodynamical equilibrium constant K_(11)~0=0.0044 for the reaction SiO_4~(4-)+SiO_4~(4-)=Si_2O_7~(6-)+O~(2-) the new model is in better agreement with the experimental data on the activity in the CaO-SiO_2 melts at 1600℃ in the region of 0.412≤N_(SiO_2)≤0.450.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/69

1 Masson, C.R., Proc. R. Soc., A287 (1965) , 201,
2 Masson, C.R., J. Am. Ceram, Soc., 51 (1968) , 134.
3 Whiteway. S.G.; Smith, I.B.; Masson. C.R., Can. J. Chem., 48 (1970) , 33,
4 Masson, C.R.; Smith, I.B., Whiteway, S. G., Can J. Chem., 48 (1970) , 1456.
5 邹元燨;周继程,徐元森,赵彭年,张子青,First China-USA Bilateral Metallurgical Conference.Beijing China,1981,p.61(Pteprint);金属学报,18(1982) .127.
6 Darken. L.S.; Gurry, R.W.. Physical Chemistry of Metals, McGraw-Hill, New York, 1953 p. 340.
7 Guggenheim, E.A., Mixtures, Clarendon Press, Oxford, 1952, p. 29.
8 Barin, I.; Knacke, O., Thermochemical Properties of Inorganic Substances, Springer-Verlag, Berlin. 1973. p. 174.
9 窦士学;刘化坤,金属学报,17(1981) ,454.
10 刘洪霖;陈念贻等;私人通讯,(1983) .
No related articles found!
No Suggested Reading articles found!