| INFLUENCE OF SOLUTION TREATMENT PARAMETERS ON DISSOLUTION OF β-PHASE FOR Ni-Be-Ti ALLOYS |
| ZHUANG Yinghong; TANG Guangquan; RONG Guoqi (Guangxi University; Nanning) |
|
Cite this article:
ZHUANG Yinghong; TANG Guangquan; RONG Guoqi (Guangxi University; Nanning). INFLUENCE OF SOLUTION TREATMENT PARAMETERS ON DISSOLUTION OF β-PHASE FOR Ni-Be-Ti ALLOYS. Acta Metall Sin, 1986, 22(5): 57-62.
|
|
|
Abstract The influences of solution treatment and Ti content on the dissolution behaviour of β-phase in Ni-Be-Ti alloys were studied by techniques of optical microscopy, DTA and EMPA. Plots of the dissolution rate of β-phase against solution treatment parameters were made quantitatively. The dissolution process ofβ-phase in this alloy was elucidated in the light of the data obtained.
|
|
Received: 18 May 1986
|
1 Kawacki Berylco Industries Inc., Berylco Nickel Alloys 440, Alloy Digest, Publ. by Eng, Alloys Digest Inc., Upper Montclair, New Jersey, Revised Sept. 1975. 2 村上陽太郎,日本金属学会会报,13(1974) ,479. 3 湯广权;荣国器,卢美德;孙精勤,庄应烘,广西大学学报,待发表. 4 Jahn, E.Z., Z. Metallk., 40 (1949) , 399. 5 Aldinger, F.; Petzow, G., Beryllium Science and Technology, Vol. 1, Eds. Webster, D.; London, G. J., Plenum Press, New York, 1979, p. 235.% |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|