Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (5): 53-150    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF GRAIN SIZE ON SLOW FATIGUE CRACK PROPAGATION AND PLASTIC DEFORMATION ZONE OF CRACK TIP
DENG Rongying; YU Guiqing; LI He (Institute of Mechanics; Academia Sinica; Beijing)
Cite this article: 

DENG Rongying; YU Guiqing; LI He (Institute of Mechanics; Academia Sinica; Beijing). EFFECT OF GRAIN SIZE ON SLOW FATIGUE CRACK PROPAGATION AND PLASTIC DEFORMATION ZONE OF CRACK TIP. Acta Metall Sin, 1986, 22(5): 53-150.

Download:  PDF(1999KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fatigue crack propagation threshold and slow propagation near it were studied at the constant amplitude of the cyclic load ratio, R=0.5 for three-point bend specimen of the austenite stainless steel. The effect of grain size on the plastic deformation of crack tip at the threshold and at slow propagation near it were investigated using the relief method. The results show that the threshold value of crack propagation increases linearly with the square root of grain size and the rate was slower for larger grain sized material. The proportionality factors of plastic deformation zone size of crack tip and (K_(max)/σ_z)~2 for various grain size are different at the threshold. The larger the grain size, the larger is the proportionality factor. At the same time, the distinction of the plastic deformation development is the uncontinuous and unsymmetric as da/dN is from 2×10~(-8)-10(-7)mm/cyc. A dimensionless criterion of crack starting propagation, n(△K_(th)/2σ_sd~(1/2)) which is constant for various grain size was obtained after the results of the test were put in order. Its physical significance is that fatigue crack starts to propagate when the square root of the ratio of the cyclic plastic zone size and grain size equals 0.6. The metallographic and SEM observations show that the crack propagation near the threshold of austenite stainless steel proceeds on the transgranular shear mode cyclic cleavage and plasticity tear.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/53

1 郑哲敏,力学进展,12(1982) ,№ 2,133.
2 Nakai, Y.; Tanaka, K., Eng. Fract. Mech., 15 (1981) , 291.
3 Higo, Y.; Pickard, A.C.; Knott, J.F., Met. Sci., 15 (1981) , 233.
4 Robin, C.; Pluvinage, G., Mater. Struct., 3 (1980) , 287.
5 邓蓉英;李禾;于桂清,金属学报,20 (1984) ,A76.
No related articles found!