A MATHEMATICAL MODEL FOR FLUID FLOW IN MOLTEN BATH AGITATED BY IMPINGING GAS JET
DU Cichen; ZHANG Jiayun; WEI Shoukun (Beijing University of Iron and Steel Technology)
Cite this article: 

DU Cichen; ZHANG Jiayun; WEI Shoukun (Beijing University of Iron and Steel Technology). A MATHEMATICAL MODEL FOR FLUID FLOW IN MOLTEN BATH AGITATED BY IMPINGING GAS JET. Acta Metall Sin, 1986, 22(5): 137-139.

Download:  PDF(237KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new boundary condition of the vorticity on the surface of the cavity caused by an impinging gas jet has been derived. The relationship between the flow field of the liquid and the impinging jet is then established. Comparing with the previous works, the velocity distributions of the flow fields are in better agreement with the experimantal results meastared.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/137

1 Szekely, J.; Asai, S., Metall. Trans., 5(1974) , 463.
2 李有章;李顶宜,北京钢铁学院院报,(1983) ,№4,48.
3 张家芸;杜嗣琛;魏寿昆,顶吹气体射流冲击下熔池流场的数学模型,中国金属学会第五届冶金过程物理化学年会论文集,下册,1984,P.11.
4 Fischer, H.B.; List, E.J.; Koh, R.C.Y.; Brooks, N.H., Mixing in Inl and andCoastal Waters, Academic Press, New York, 1979, Chapter 9.P
No related articles found!
No Suggested Reading articles found!