MECHANISM OF DECOMPOSITION OF BARITE IN PROCESS OF SINTERING JIUQUAN BARITECONTAINING IRON ORE CONCENTRATE
by REN Yunfu; FENG Lin (Beijing University of Iron and Steel Technology)
Cite this article: 

by REN Yunfu; FENG Lin (Beijing University of Iron and Steel Technology). MECHANISM OF DECOMPOSITION OF BARITE IN PROCESS OF SINTERING JIUQUAN BARITECONTAINING IRON ORE CONCENTRATE. Acta Metall Sin, 1986, 22(4): 86-92.

Download:  PDF(1677KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The study was carried out on the decomposition mechanism of barite in the sintering mixtures of Jiuquan barite-containing iron ore concentrate during sintering, and on the interaction between barite and other constituents It showed that the decomposition of barite in sintering mixtures started at 1190℃ in air, and reached its maximum rate at 1240℃ During sintering, the decomposition mechanism of barite is the solid-state reaction between barite and Fe_2O_3 which takes place at high temperatures and the product under oxidized atmosphere is BaO.6Fe_2O_3 For the sintered Jiuquan sintering mixtures the product is (BaO. 6Fe_2O_3). 1.81 (CaO.2Fe_2O_3) The apparent activation energy of barite decomposition in air is 119.9 kJ/mol and the order of reaction is 1.3—1.4 obtained by kinetical calculation.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/86

1 Van Hook, H.J., J. Am. Ceram. Soc., 47 (1964) , 580.
2 Krug, D.; Beer, F., Thermal Analysis, Budapest, July, 1974, Ed. Buzas, I., Akademidi Kiado, Hungary, Vol. Ⅰ, 1975, p. 1021-1029.
3 #12
4 叶大伦,实用无机物热力学数据手册,冶金工业出版社,1981.
5 Margrave, J.L., J. Chem. Educ., 32 (1955) , 520.
6 Freeman, E.S.; Carroll, B., 1. Phys. Chem., 62 (1958) , 395.
7 Wendlandt, W.W., Thermal Methods of Analysis, Interscience, New York, London,1968. p32-33.
8 #12
9 Ezz, S.Y.;Shehata, K.A.; Seoudi, E.A., Met. Min. Rev., 9 (1970) , 3
No related articles found!
No Suggested Reading articles found!