RELATIONSHIP BETWEEN REDUCIBILITY AND HIGH TEMPERATURE PROPERTIES OF TITANIA-RICH SLAGS |
by CUI Shuxian; QU Peixun; LI Jizong; LIU Qin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
by CUI Shuxian; QU Peixun; LI Jizong; LIU Qin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). RELATIONSHIP BETWEEN REDUCIBILITY AND HIGH TEMPERATURE PROPERTIES OF TITANIA-RICH SLAGS. Acta Metall Sin, 1986, 22(4): 93-101.
|
Abstract Study was carried out of the reducibility of titania-rich slags with relation to their high temperature properties under heating stage microscope The temperatures of fusibility and fluidity of the slags sampled at intervals of reduction smelting increase steppedly with decreasing FeO content and increasing reducibility In both ranges of 22.21>FeO wt-%>12.68, 0FeO wt-%>5 44, 0.11
|
Received: 18 April 1986
|
1 Haoenmwler. P., Ann. Chim., 7 (1962) , 513. 2 Jones, D.G.; Stephens, J.F., J. Micros., 99 (1973) , 237. 3 Sommerville, I.D.; Bell, H.B., Can. Metall. Q., 21 (1982) , 145. 4 #122 |