AN EM STUDY OF CARBIDE PRECIPITATES IN HK40 REFRACTORY STEEL
by QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang); WANG Dehe; CAO Zhiben (Dalian Institute of Technology)
Cite this article: 

by QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang); WANG Dehe; CAO Zhiben (Dalian Institute of Technology). AN EM STUDY OF CARBIDE PRECIPITATES IN HK40 REFRACTORY STEEL. Acta Metall Sin, 1986, 22(4): 67-154.

Download:  PDF(2303KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A thin foil electron microscopic study has been made of the various morphologies and microstructures of the carbides Cr_7C_3 and M_(23)C_6 in HK40 (4Cr25-Ni20) austenite casting steels The orientation relationship between the M_(23)C_6 precipitates and the austenite matrix during high temperature tempering has been identified by electron diffraction patterns The morphologies and Burgers vectors of the dislocations in the austcnite matrix, carbides and interfaces have been examined The weak beam and Moire pattern techniques have also been used in the analysis
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/67

1 Terao, N.; Sasmal, B., Metallography, 13 (1980) , 117.
2 Lewis, M.; Hattersley, B., Acta Metall., 13 (1965) , 1159.
3 Beckitt, F.R.; Olark, B.R., Acta Metall., 1$ (1967) , 113.
4 Pumphrey, P.H.; Edington, J.W., Acta Metall., 22 (1974) , 89.
5 Nilsson, J.O.; Dunlop, G.L., J. Micros., 115 (1979) , 235.
6 西野知良,贺川直彦,铁钢,58(1972) ,107.
No related articles found!
No Suggested Reading articles found!