ELECTRICAL RESISTANCE MINIMA THEORY OF CuNi ALLOY
by YANG Zhenfan (Department of Physics; Wuhan University); LIU Fusui (Department of Physics; Peking University)
Cite this article: 

by YANG Zhenfan (Department of Physics; Wuhan University); LIU Fusui (Department of Physics; Peking University). ELECTRICAL RESISTANCE MINIMA THEORY OF CuNi ALLOY. Acta Metall Sin, 1986, 22(4): 63-66.

Download:  PDF(266KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electrical resistivity of paramagnetic CuNi alloys in composition range between 30 and 42 at.-% Ni due to spinflip scattering of conduction electrons from individual and coupled spin-clusters was studied by using the disordered spin-cluster model Together with the ρ_L(T) phonon contribution, the total resistivity can be written as: ρ=ρ_L(T)+ρ_0(0)-nρ_1lgT+A n~2/T The resistance minima that was observed in the experiments was explained by using the results.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/63

1 Kondo, J., Progr. Theoret. Phys., (Kyoto), 32 (1964) , 37.
2 Houghton, R.W.; Sarachik, M.P.; Kouvel, J.S., Solid State Commun., 8 (1970) , 943.
3 Yu Mei; Tyler E.H.; Luo, H.L., Phys. Rev., B26 (1982) , 4299.
4 Eno, H.F.; Tyler, E.H.; Luo, H.L.,J. Low Temp. Phys., 28 (1977) , 443.
5 Levin, K.; Mills, D., Phys. Rev., B9 (1974) , 2354.
6 Liu, Fu-sui; Ruvalds, J., Physics, 107B (1981) , 623
No related articles found!
No Suggested Reading articles found!