Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (4): 59-62    DOI:
Current Issue | Archive | Adv Search |
STRESS INDUCED TRANSFORMATION IN SUPERELASTIC NiTi ALLOY
by JIN Jialing; ZHANG Yi (Shanghai Institute of Iron and Steer Research)
Cite this article: 

by JIN Jialing; ZHANG Yi (Shanghai Institute of Iron and Steer Research). STRESS INDUCED TRANSFORMATION IN SUPERELASTIC NiTi ALLOY. Acta Metall Sin, 1986, 22(4): 59-62.

Download:  PDF(1404KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The process of stress induced transformation in 51.6 at-%Ni-Ti alloy has been studied by means of X-ray diffraction and TEM equipped with loading attachment The results show that the process may proceed as two stages: premartensitie and martensitie transformations It seems to be reversible with unloading
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/59

1 金嘉陵,金属学报,20(1984) ,A176.
2 徐祖耀,马氏体相变与马氏体,科学出版社,1980,p.502.
3 Perkins, J., Metall. Trans., 4 (1973) , 2709.
4 De Lange, R.G.; Zijderveld, J.A., J.Appl. Phys., 39 (1968) , 2195.
No related articles found!