POSITRON ANNIHILATION IN Fe_(38)Ni_(40)Mo_4B_(18) GLASS
by YU Weizhong; GU Binglin; CAO Bisong (Department of Physics; Tsinghua University; Beijing); FENG Pingyi; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Siniea)
Cite this article:
by YU Weizhong; GU Binglin; CAO Bisong (Department of Physics; Tsinghua University; Beijing); FENG Pingyi; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Siniea). POSITRON ANNIHILATION IN Fe_(38)Ni_(40)Mo_4B_(18) GLASS. Acta Metall Sin, 1986, 22(4): 136-137.
Abstract The positron life-time spectra in Fe_(38)Ni_(40)Mo_4B_(18) glass at different temperatures have been measured and the annihilation mechanism has been discussed.