by FENG Zhimin; FU Yulan; ZHAO Keqing (Research Institute of Anshan Iron and Steel Company)
Cite this article:
by FENG Zhimin; FU Yulan; ZHAO Keqing (Research Institute of Anshan Iron and Steel Company). REMEDY FOR FISHSCALE ON ENAMEL STEEL SHEET. Acta Metall Sin, 1986, 22(4): 133-135.
Abstract The tendency to fishscale on the enamel steel sheets of TC_1, 08F, 08Al, etc. has been investigated by the electrochemical H-permeation method. It showed that the fishscaling is closely related to the diffusion coefficient of hydrogen in steel. With the increase of the deformation and the Ti/C ratio of steel, the diffusion coefficient of hydrogen may be decreased and thus its tendency to fishscale may be also decreased.