Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (4): 131-132    DOI:
Current Issue | Archive | Adv Search |
REMOVAL OF NON-METALLIC INCLUSION FROM ALLOY 0Cr25A15 BY ELECTROSLAG REMELTING
by MENG Qingying (Jinzhou Institute of Technology)
Cite this article: 

by MENG Qingying (Jinzhou Institute of Technology). REMOVAL OF NON-METALLIC INCLUSION FROM ALLOY 0Cr25A15 BY ELECTROSLAG REMELTING. Acta Metall Sin, 1986, 22(4): 131-132.

Download:  PDF(171KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of the slag system and addtive, including alloying element and deoxidizer, on the non-metallic inclusion removal from the electrothermal alloy 0Cr25A15 in the process of the electroslag remelting has been examined. The choice of slag system containing RE, the addition of Al as deoxidizer and the use of consumable electrode free from Ti are found to be the favourable conditions for remelting technique.
Received:  18 April 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I4/131

1 孟庆应,锦州工学院学报,(1983) ,No.2,87.
No related articles found!