| EQUILIBRIA OF Ce-Al-O AND Nd-Al-O IN MOLTEN IRON |
| DIAO Shusheng; HAN Qiyong; LIN Gang; CHEN Dong (Beijing University of Iron and Steel Technology) |
|
Cite this article:
DIAO Shusheng; HAN Qiyong; LIN Gang; CHEN Dong (Beijing University of Iron and Steel Technology). EQUILIBRIA OF Ce-Al-O AND Nd-Al-O IN MOLTEN IRON. Acta Metall Sin, 1986, 22(2): 51-60.
|
|
|
Abstract Equilibrium of Ce-Al-O or Nd-Al-O system in molten iron was studied by separately smelting the radioactive isotope of ~(141)Ce or ~(147)Nd in an Al_2O_3 crucible filled with pure iron to form ~(141)CeAlO_3 or ~(147)NdAlO_3 around its inner wall. The content of dissolved Ce or Nd in iron was determined by means of radioassay and electrolysis in organic electrolyte. The analysis of dissolved Al in iron was obtained by colorimetry and followed by calculation. The activity of oxygen as dissolved state in liquid iron was directly measured by solid electrolyte sensors made of ZrO_2(MgO) tube. By extrapolation of data obtained, the temperature dependence of equilibrium constant of RE-Al-O in molten iron, K_(REAlO_3) or of interaction coefficient, e_(RE)~(Al), may be described as: For reaction CeAlO_(3(s)=[Ce]+[Al]+3[O] lg K_(CeAlO_3)=-37900/T+5.84 △G_(CeAlO_3)~0=175400-26.7T cal/mol e_(Ce)~(Al)=20500/T-13.53 For reaction NdAlO_(3(s)) =[Nd]+[Al]+3[O] lg K_(NdAlO_3)=-24700/T+0.69 △G_(NdAlO_3)~0=113030-3.16T cal/mol e_(Nd)~(Al)=13500/T-9.33
|
|
Received: 18 February 1986
|
1 韩其勇;吴卫江;方克明;霍成章;周小龙,中日钢铁学术会议,第一届炼钢学术会议报告,中国金属学会,北京,1981年p.25;钢铁,17 (1982) ,№2,1. 2 韩其勇;刘士伟;牛红兵;唐志伟,金属学报,18 (1982) ,176. 3 韩其勇;项长祥,董元篪;杨斯馥,日本,中国铁钢学术会议第二回制钢学术会议报告,东京,1983,p.10. 4 韩其勇;董元篪;牛锡安;项长祥;杨斯馥,金属学报,20 (1984) ,204. 5 武恩佑;陈鹏,北京钢铁学院学报,(1982) ,№2,157. 6 丰锡安,北京钢铁学院研究生论文,1979. 7 Sigworth, G.K.; Elliott, J. F., Met. Sci., 8 (1974) , 298. 8 韩其勇,北京钢铁学院学报,(1982) ,№2,157. 9 #12 10 #12 |
| No Suggested Reading articles found! |
|
|