CALCULATION OF α/γ EQUILIBRIUM PHASE BOUNDARY IN LOW ALLOY STEELS
ZHAO Yuxin; LI Pengxing; XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University)
Cite this article: 

ZHAO Yuxin; LI Pengxing; XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University). CALCULATION OF α/γ EQUILIBRIUM PHASE BOUNDARY IN LOW ALLOY STEELS. Acta Metall Sin, 1986, 22(2): 42-50.

Download:  PDF(589KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The α/γ phase boundary, relative proportion of the two phases and A temperature have been calculated by extending the Sharma et al. 's regular solution model to multicomponent commercial steels 20Cr, 30Cr, 40Cr, 40Mn2, 20CrMn, 35CrMn2, 38CrSi and 30CrMnSi with the thermodynamical data taken from available literatures. The calculated A are in good agreement with the experimental data.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/42

1 Sharma, R.C.; Purdy, G.R.; Kirkaldy, J.S., Metall. Trans.,. 10A (1979) , 1119.
2 Hillert, M.; Staffansson, L.-I., Acta Chem. Scand., 25 (1970) , 3618.
3 Nelder, J A.; Meed, R., Comput. J., 7 (1965) , 308.
4 Himmelblau,R.M.,实用非线性规则,张文桑等译,科学出版社,北京,1981年.
5 徐祖耀,金属材料热力学,科学出版社,北京,1981年,第10章.
6 Ban-Ya, S.; Elliott, J.F.; Chipman, J., Metall. Trans., 1 (1970) , 1313.
7 Harvig, H., Jernkont. Ann., 155 (1971) , 157.
8 Agreen, J., Metall. Trans., 10A (1979) , 1847.
9 kirchner, G.; Nishizawa, T.; Uhrenius, B., Metall. Trans., 4 (1973) , 167.
10 Weiss, R.J.; Tauer, K.J., Phys. Rev., 102 (1956) , 1490.
11 Wada, T.; Wada, H.; Elliott, J.F.; Chipman, J., Metall. Trans., 3 (1972) , 1657.
12 Kirchner, G.; Uhrenius, B., Acta Metall., 22 (1974) , 523.
13 Chart, T.; Putland, F.; Dinsdale, A., CALPHAD, 4 (1980) , 27.
14 赵宇新,上海交通大学硕士论文,1984年.
15 合金钢钢种手册,第一册,合金结构钢,冶金工业出版社,北京,1983年.
16 合金钢手册,下册,中国工业出版社,北京,1964年
No related articles found!
No Suggested Reading articles found!