CORRELATION BETWEEN STRUCTURE OF ELECTROCHEMICALLY DEPOSITED (Fe,Co,Ni)-P LAYERS AND PROCESS CONDITIONS
JIANG Xiaoxia; ZHANG Xuan; LIN Shuzhi (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

JIANG Xiaoxia; ZHANG Xuan; LIN Shuzhi (Institute of Metal Research; Academia Sinica; Shenyang). CORRELATION BETWEEN STRUCTURE OF ELECTROCHEMICALLY DEPOSITED (Fe,Co,Ni)-P LAYERS AND PROCESS CONDITIONS. Acta Metall Sin, 1986, 22(2): 124-133.

Download:  PDF(2999KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study has been made of the structure of the electrochemically deposited amorphous (Fe, Co, Ni)-P layers with relation to the process conditions, e.g. pH value, current density, metallic salt concentration, etc., by means of X-ray analysis, SEM and EPMA. Results showed that the effect of the process on the structure is realized by changing the P content of the layer. While P contained over 8%, below 3% or between 3 and 8%, a layer may be constructed as amorphous alloy, supersaturated solution or mixed structures respectively. The major factors affecting the structure of the deposited layer are found to be the concentration of NaH_2PO_2 and pH value of the bath. The structure of the layer may be also influenced by the potential of electro-deposition. The Fe-P, Co-P or Ni-P system is similar in amorphous structure of which the highest thickness of stack of the atomic face is 2.0, 2.5 or 6.5nm respectively.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/124

1 石桥知;鹰野修;青木公二,金属表面技术,21 (1970) ,541;31 (1980) ,28.
2 Brenner, A., J. Res. Nat. Bur. Stand., 44 (1950) , 109.
3 增井宽二,日本金属学会誌,41 (1977) ,1130.
4 #12
5 #12
6 云南省交通科学研究所,镀铁电镀液研究,1970.
7 武汉锅炉厂403车间,防腐包装,1979.
8 渡(刀辶)徹,金属表面技术,32 (1981) ,601.
9 吉岡正三,金属表面技术,20 (1961) ,172.
10 林树智;黑祖昆,物理学报,33 (1984) ,302.
11 Dixmier, J.; Gunier, A., Rev, Metall,, (Paris), 64 (1967) , 53.[
No related articles found!
No Suggested Reading articles found!