A NEW METHOD FOR MEASURING DENSITY OF HIGH TEMPERATURE MELT
BIAN Maoshu; MA Luming; WANG Jingtang (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

BIAN Maoshu; MA Luming; WANG Jingtang (Institute of Metal Research; Academia Sinica; Shenyang). A NEW METHOD FOR MEASURING DENSITY OF HIGH TEMPERATURE MELT. Acta Metall Sin, 1986, 22(2): 134-140.

Download:  PDF(583KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  According to Archimedes principle, a method, so called couple weighing method, for measuring the density of the high temperature melt was proposed in which a new-designed sinker, corresponding measuring regime and calculating formula are presented. Examples of the simultaneous measurement under similar conditions are shown that the data collected by this method with more accuracy and precision than that by both methods of Archimedes correction and bi-sinker.
Received:  18 February 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I2/134

1 Kirshenbaum, A.D.; Cahill, J.A.; Grosse, A.V., J. Inorg. Nucl. Chem., 24 (1962) , 333.
2 Bertheu, P.E.; Tougas, R., J. Less-Common Met., 16 (1968) , 465.
3 饭田孝道;深赖昭二;森田善一郎,日本金属学会会报,20 (1981) ,264.
4 森田善一郎;荻野善清;垣内博之;足立彰,日本金属学会誌,34 (1970) ,248.
5 #12
6 冯师颜编,误差理论与实验数据处理,科学出版社,1969.
7 Cahill, J.A.; Kirshenbaum, A.D., J. Inorg. Nucl. Chem., 26 (1964) , 206; J. Phys. Chem., 66 (1962) , 1080.
8 Bornemann, K.; Saurwald, F., Z. Metallk., 14 (1922) , 145.
9 Kirshebaum, A.D.; Cahill, J.A., ASM Trans. Q., 55 (1962) , 844.
10 Pascal, P.; Jouniaux, A., Compt. Rend. Acad. Sci., 158 (1914) , 414.
11 Pluss, M., Z. Anorg. Allg. Chem., 91 (1919) , 106.
12 Sosman, R.B.; Day, A.L.; Hostetter, J.C., Am.J. Sci., 1 (1914) , 37.
13 Matuyama, Y., Sci. Repts. Tohoko, Imp. Univ., 1st Ser., 18 (1929) , 19.
14 #12
No related articles found!
No Suggested Reading articles found!