Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (5): 37-142    DOI:
Current Issue | Archive | Adv Search |
STRESS-STRAIN BEHAVIOUR AND MICROSTRUCTURE OF NiTi SHAPE-MEMORY ALLOY
ZHANG Yi;JIN Jialing Shanghai Institute of Iron and Steel Research
Cite this article: 

ZHANG Yi;JIN Jialing Shanghai Institute of Iron and Steel Research. STRESS-STRAIN BEHAVIOUR AND MICROSTRUCTURE OF NiTi SHAPE-MEMORY ALLOY. Acta Metall Sin, 1985, 21(5): 37-142.

Download:  PDF(2935KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The stress-strain plot and microstructure of 51.6 at.-% Ni-Ti shape-memory alloywere examined and observed under different heat treatments.The phenomena andpossible machanism o f Premartensitic transition,the morphology and substructureof martensite induced by temperature or strain as well as the dispersed χ-phase pre-cipitation of the alloy were also discussed.
Received:  18 May 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I5/37

1 金嘉陵,金属学报,20(1984) .
2 金嘉陵等,待发表工作.
3 Aborlfotoh,M.O.;Aboelfotoh,H.A.;Washburn,J.,J.Appl.Phys.,40(1978) ,5230.
4 Wasilewski,R.J.;Butler,S.R.;Hanlon,J.E.,Met.Sci.,J.,1(1967) ,104.
5 Kolomytsev,V.I.;Lobodyuk,V,A.;Khandros,L.G.,Phys.Status Solidi,(a)50(1978) ,127.
6 Kolomytsev;V.I.;Lobodyuk,V.A.;Khandros,L.G.,Phys.Status Solidi,(a)65(1981) ,87.l
No related articles found!
No Suggested Reading articles found!