Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (4): 95-104    DOI:
Current Issue | Archive | Adv Search |
STRUCTURAL RELAXATION AS THE ORIGIN OF MAGNETIC PERMEABILITY DECAY IN AMORPHOUS ALLOY Fe_(76)Si_(10)B_(14)
ZHANG Yanzhong Shanghai Iron and Steel Research Institute
Cite this article: 

ZHANG Yanzhong Shanghai Iron and Steel Research Institute. STRUCTURAL RELAXATION AS THE ORIGIN OF MAGNETIC PERMEABILITY DECAY IN AMORPHOUS ALLOY Fe_(76)Si_(10)B_(14). Acta Metall Sin, 1985, 21(4): 95-104.

Download:  PDF(792KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Kinetics of the magnetic permeability decay of an amorphous alloy Fe_(76)Si_(10)B_(14)at temperature range of 50-300℃ was examined.The evidence of isochronalstructural relaxation spectra as the origin of the magnetic permeability decay wasobtained.The most probable activation energy and the distribution of activationenergy were calculated.By using the two-level-one-configuration model developedby Kronmüller,the reversibility of this type of relaxations was discussed.Theorigin of the decay was also analyzed.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/95

1 Matsuyama,T.;Ohta,K.;Kajiura,M.;Teranishi,T.,Jpn.J.Appl.Phys.,19(1980) ,55.
2 Nose,M.;Esashi,K.;Kanrhira,J.;Ohnuma,S.;Shirakawa,K.;Masumoto,T.,Proc.4th Int.Conf.on Rapidly Quenched Metals,Eds.Masumoto,T.;Suzuki,K.,Vol.1,The Jpn Inst.Met.,1982,p.1191.
3 张延忠;程东;张东平,金厲学报,(待发表).
4 Fish,G.E.;Ramanan,V.R.V.;Hasegawa,R.;Diebild A.C.,IEEE Trans.Magn.,MAG-19(1983) .1937.
5 Morito,N.;Egami,T.,ibid.,MAG-19(1983) ,1898.
6 Flanders,P.J.;Morito,N.;Egami,T.,ibid.,MAG-19(1983) ,1907.
7 Egami,T.,J.Magn.Magn.Mater.,31-34(1983) ,1571.
8 Phillips,D.L.,J.Assoc.Mach.,9(1962) ,84.
9 Hesse,J.;Ruebartsch,A.,J.Phys.,E 7(1974) ,526.
10 王梓坤,概率论基础及其应用,科学出版社,北京,1979,p.82.
11 Miyazaki,T.;Hisatake,K.;Takahashi,M.,Jpn.J.Appl.Phys.,22(1983) ,1277.
12 Miyazaki,T.;Takahashi,M.,J.Magn.Magn.Mater.,42(1984) ,29.
13 Kneller,E.,Ferromagnetsmus,Springer-verlag,Berlin/Gottingen/Heidelberg,1962,p.376.
14 Kronmueller,H.,Philos.Mag.,B 48(1983) ,127.
15 Kronmueller,H.,J.Magn Magn.Mater.,41(1984) ,366.
16 Boerner,H.;Hoehne,R.,Phys.Status Solidi,(a)76(1983) ,499.g
No related articles found!
No Suggested Reading articles found!