Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (4): 89-94    DOI:
Current Issue | Archive | Adv Search |
TEMPERATURE DEPENDENCE OF ELECTRICAL RESISTIVITY OF SOME AMORPHOUS ALLOYS
FENG Benzheng;YANG Rusen Institute of Precious Metals Kunming
Cite this article: 

FENG Benzheng;YANG Rusen Institute of Precious Metals Kunming. TEMPERATURE DEPENDENCE OF ELECTRICAL RESISTIVITY OF SOME AMORPHOUS ALLOYS. Acta Metall Sin, 1985, 21(4): 89-94.

Download:  PDF(375KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Measurements of the electrical resistivity,its temperature dependence and the tran-sition temperatures at different stages of some amorphous alloys,such as Zr_(100-x)M_x(M=Fe,Co,Ni,Cu or Pd),Cu_(100-x)Ti_x,Pd_(83.5-x)Si_(16.5)M_x(M=Cu,Ag,Ni,Pt,Rh,Ru,Ir,Os,Hf,Ta,W or Re)and Pd_(80-x)Si_(20)Cr_x prepared by the meltspinningtechnique were made in the temperature range of 0—500℃.The effects of minoradditives on them are also discussed.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/89

1 Gallagher,B.L.;Greig,D.;J.Phys.,F.12(1982) ,1721.
2 Budhani,R.C.;Goel,T.C.;Chopra,K.L.,J.Phys.,F,13(1983) ,129.
3 Bushow,K.H.J.;Beekman,N.M.,Phys.Rev.,B,19(1979) ,3843.
4 Fritsch,G.;Willer,J.;Luescher,E.,J.Non-Cryst.Solids,46(1981) ,321.
5 Hwang,C.H.,J.Less-Common Met.,86(1982) ,187.
6 冯本政;朱应华;杨汝森,金属学报,20(1984) ,B 224.
No related articles found!
No Suggested Reading articles found!