STRUCTURE OF ELECTRODEPOSITED Ni-Mo OR Ni-W ALLOY
HEI Zukun;LI Jinghuan;LIN Shuzhi Institute of Metal Research;Academia Sinica;Shenyang
Cite this article: 

HEI Zukun;LI Jinghuan;LIN Shuzhi Institute of Metal Research;Academia Sinica;Shenyang. STRUCTURE OF ELECTRODEPOSITED Ni-Mo OR Ni-W ALLOY. Acta Metall Sin, 1985, 21(4): 21-26.

Download:  PDF(484KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of plating factors on the structure of electrodeposited.Ni-Mo orNi-W alloy has been studied.It was found that the pH value is a decisive oneamong factors whether the deposited alloy can be made or not as amorphous struc-ture.The changes in the structure still seem to be explained by the model pre-viously developed by the authors to interpret the structure of the Ni-P depositedlayer.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/21

1 Aur,S.;Kofalt,D.;Waseda,Y.;Egami,T.;Chen,H.S.;Teo,B.K.;Wang,R.,J.Non-Crystal Solid,61/62(1984) ,331.
2 今永広人,金属表面技术,19(1968) ,73.
3 今永広人,工业化学杂志,67(1964) ,803.
4 渡边彻;田边良美,金属表面技术,32(1981) ,600.
5 小见崇;山本文;金属表面技术,29(1978) ,460.
6 东敬;福岛久哲,日本金属学会会报,13(1974) ,645.
7 Mamadou Diehiou,Thesis Centre d' Etudes de Chimie Metallurgigue,1983.
8 小见崇,金属表面技术,31(1980) ,85.
9 Pearson,W.B.,A Handbook of Lattice Spacings and Structures of Metals and Alloys,Pergamon Press,New York,1958,p.754.
10 榷尾一,清水辉夫,金属表面技术,19(1968) ,64.
11 林树智,黑祖昆,物理学报,33(1984) ,302.
12 Warren,B.E.,Phys.Rev.,59(1941) ,693.
No related articles found!
No Suggested Reading articles found!