ELECTRICAL PROPERTIES AND CRYSTALLIZATION OF Cu_(0.60)Ti_(0.40)METALLIC GLASS
ZHOU Xinming Institute of Precious Metals;Ministry of Metallurgical Industry;Kunming
Cite this article: 

ZHOU Xinming Institute of Precious Metals;Ministry of Metallurgical Industry;Kunming. ELECTRICAL PROPERTIES AND CRYSTALLIZATION OF Cu_(0.60)Ti_(0.40)METALLIC GLASS. Acta Metall Sin, 1985, 21(4): 120-127.

Download:  PDF(487KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electrical properties and crystallization of Cu_(0.60)Ti_(0.40)metallic glass wereinvestigated by X-ray diffraction,DSC technique and electrical resistance measure-ment under isothermal and isochronal heating conditions.A negative temperaturecoefficient of electrical resistivity of the metallic glass Cu_(0.60)Ti_(0.40)is presented,andit becomes positive and increasing value in process of crystallization.Its crystal-lization is shown in two stages and in conformity with he J-M-A equationbasically.A good mutual couforment about the activation energies of crystalliza-tion was made with calculation by various methods.It seems that there is agreat potentiality in the increase of the stability of Cu-Ti metallic glass.
Received:  18 April 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I4/120

1 Maeland,A.J.;Hydrides for Energy Storage,Eds.Anderson,A.F.;Maeland,A.J.,Pergamon Press,Oxford,1978,p.447.
2 Marshall,A.F.;Lee,Y.S.;Stevenson,D.A.,Acta Metall.,31(1983) ,1225.
3 高逸群;周新铭;邓德国,金属玻璃中的动力学问题,昆明贵金属研究所,1980.
4 Henderson,D.W.,J.Non-Cryst.Solids,30(1979) ,301.
5 Buschow,K.H.J.,Acta Metall.,31(1983) ,155.
6 Hwang Chall-Hong;Ryeom Yeong-Jo;Cho Kangjo,J.Less-Common Met.,86(1982) ,187.
No related articles found!
No Suggested Reading articles found!