EFFECT OF QUENCHING TEMPERATURE ON MORPHOLOGY OF MARTENSITE IN T12 STEEL |
LIU Changze Wuhan Institute of Iron and Steel Technology |
|
Cite this article:
LIU Changze Wuhan Institute of Iron and Steel Technology. EFFECT OF QUENCHING TEMPERATURE ON MORPHOLOGY OF MARTENSITE IN T12 STEEL. Acta Metall Sin, 1985, 21(3): 83-86.
|
Abstract The effect of the different quenching temperatures,780-1050℃,on the mor-phology of martensite formed under different temperatures in T12 steel has beenstudied by optical and electron microscope.It is believed that the microstructureof T12 steel quenched from elevated temperature seems to be quite complex.
|
Received: 18 March 1985
|