EFFECT OF Nb ON LONG-TIME AGING STABILITY OF AN AUSTENITIC HEAT RESISTING STEEL 37Mn31Al3Cr2MoVWNbB
ZHANG Futian; SU Lijuan; ZHANG Yanshen (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 8 November; 1983)
Cite this article: 

ZHANG Futian; SU Lijuan; ZHANG Yanshen (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 8 November; 1983). EFFECT OF Nb ON LONG-TIME AGING STABILITY OF AN AUSTENITIC HEAT RESISTING STEEL 37Mn31Al3Cr2MoVWNbB. Acta Metall Sin, 1984, 20(6): 411-493.

Download:  PDF(3143KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of Nb content on the long-time aging stability in hot strength and structure of an austenitic heat resisting steel 37Mn31Al3Cr2MoVWNbB has been investigated. It was found that the hot strength of the steel is no longer decreased and the structural stability is dependent on the shape and distribution of NbC after long-time aging at 650℃. The coarse prior NbC deteriorates the structural stability and promotes the decomposition of matrix and the growth of x-phase which embrittles the steel. Thus, it seems to be considered to cut down the Nb content in the steel.
Received:  18 June 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I6/411

1 张彦生;王明贤;赵学军;许义奎;朴凯东,钢铁17(1982) ,No.4,45.
2 张彦生;张弗天;高会友;王根元,金属学报,20(1984) ,A1.
3 Heikkinen, V. K.; Packwood, R. H., Scand. J. Met., 6 (1977) , 170.
4 Guha, J. P.; Kolar, D., J. Less-Common Met., 29 (1972) , 33.
5 刘嘉乐;庄育智;金属学报,5(1960) ,24.
6 管恒荣;黄有山;楼翰一;白林祥;中国腐蚀与防护学报,2(1982) ,No.2,11.
7 Vodopivec, F.; Gabrovsek, M.; Ralic, B., Met. Sci., 9 (1975) , 324.
8 Fletcher, E. E.; Elsea, A. R.; Bain, E C., ASM Trans. Q., 54 (1961) , 1.
No related articles found!
No Suggested Reading articles found!