APPLICATION OF TWO-DIMENSIONAL BINARY SYSTEM TO STUDY CERTAIN PHASE DIAGRAMS
DU Yijing; CHEN Lirong; YAN Zutong (Department of Physics; Anhui Normal University; Wuhu) (Manuscript received 16 May; 1983; revised manuscript 23 September; 1983)
Cite this article: 

DU Yijing; CHEN Lirong; YAN Zutong (Department of Physics; Anhui Normal University; Wuhu) (Manuscript received 16 May; 1983; revised manuscript 23 September; 1983). APPLICATION OF TWO-DIMENSIONAL BINARY SYSTEM TO STUDY CERTAIN PHASE DIAGRAMS. Acta Metall Sin, 1984, 20(5): 422-430.

Download:  PDF(440KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To extend the Collins' model of two-dimensional system into binary substitutional system, its Gibbs' function and free energy may be evaluated and then the equation for determination of binary phase equilibrium curve may be obtained. Certain common phase diagrams were investigated, as well as a concrete calculation was made of the "cigar" phase diagram. The obtained results are quite analogous to the behaviour of the three-dimensional ones.
Received:  18 May 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I5/422

1 Collins, R. , Proc. Phys. Soc. , 83 (1964) , 553.
2 杜宜瑾;陈立溁;严祖同,物理学报,31(1982) ,939.
3 杜宜瑾;陈立溁;严祖同,物理学报,32(1983) .96.
4 #121
No related articles found!
No Suggested Reading articles found!