A NOTE ON IMPROVEMENT OF CONTACT FATIGUE LIFE OF BEARING STEEL BY RARE EARTH
XU Chuancai; ZHANG Longshui (Xi'an Institute of Metallurgical Architecture) (Manuscript received 3 August; 1982; revised manuscript 7 November; 1983)
Cite this article: 

XU Chuancai; ZHANG Longshui (Xi'an Institute of Metallurgical Architecture) (Manuscript received 3 August; 1982; revised manuscript 7 November; 1983). A NOTE ON IMPROVEMENT OF CONTACT FATIGUE LIFE OF BEARING STEEL BY RARE EARTH. Acta Metall Sin, 1984, 20(4): 303-304.

Download:  PDF(141KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to improve the contact fatigue life of the bearing steel, the rare earth was used as deoxidizer partly instead of Al in the conventional processing. This RE ladle deoxidizer in amount of 0.08 wt-% of the melt produces inclusions of Ce_2S_3, CeS, La_2S_3, etc. which tend to increase the fatigue life of the steel by 50%.
Received:  18 April 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I4/303

No related articles found!
No Suggested Reading articles found!