| A NEW SPHEROIDIZATION PROCESS FOR HIGH-SULPHUR MOLTEN IRON |
| ZHU Yuanka; PENG Yujiang; HONG Yanruo; SU Liuji; YU Xuebin (Beijing University of Iron and Steel Technology) (Manuscript received 7 March; 1983; revised manuscript 31 October; 1983) |
|
Cite this article:
ZHU Yuanka; PENG Yujiang; HONG Yanruo; SU Liuji; YU Xuebin (Beijing University of Iron and Steel Technology) (Manuscript received 7 March; 1983; revised manuscript 31 October; 1983). A NEW SPHEROIDIZATION PROCESS FOR HIGH-SULPHUR MOLTEN IRON. Acta Metall Sin, 1984, 20(4): 305-312.
|
|
|
Abstract A new spheroidization process was developed for production of nodular cast iron from high-sulphur (0.1%S) molten iron. The solid slag cake of rare-earth oxide was used as desulphurizer and spheroidizer under the Ar-blowing operation. The results achieved after the experiments under 1380, 1410 or 1450℃. Treatment at 1450℃ for about 45 min attended 90% of success. The carbon equivalent and the content of rare-earth for nodular cast iron produced are about 4.7% and 0.020—0.081% respectively. Thermodynamic analysis on the desulphurization and the reduction of rare-earth oxides has proved available for the experimental conditions. And it was indicated by both thermodynamic calculation and experimental practice that the solid slag cake may be used repeatedly.
|
|
Received: 18 April 1984
|
1 朱元凯;彭(忄育)强;洪彦若;李联生;杨广禄,稀土,4(1983) ,12. 2 Strizik, P.; Jeglish, F., Int. Cast Met. J., 1 (1976) , №3, 23. 3 Lux, B., Cast Met. Res. J., 8 (1972) , №2, 49. 4 Vahed, A.; Kay, D. A. R., Metall. Trans., 7B (1976) , 375. 5 魏寿昆,冶金过程热力学,上海科学技术出版社,1980,p.16.T |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|