IMPACT FRACTURE BEHAVIOUR OF 09MnNb STEEL AT LOW TEMPERATURES
by CAI Tikang; LI Peiliang; JIANG Jingkai (Baotou Institute of Metallurgy) (Manuscript received 10 January; 1981; revised manuscript 4 December; 1982)
Cite this article: 

by CAI Tikang; LI Peiliang; JIANG Jingkai (Baotou Institute of Metallurgy) (Manuscript received 10 January; 1981; revised manuscript 4 December; 1982). IMPACT FRACTURE BEHAVIOUR OF 09MnNb STEEL AT LOW TEMPERATURES. Acta Metall Sin, 1983, 19(4): 88-152.

Download:  PDF(3273KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The low-temperature impact fracture of controlled-rolled and normalized steel 09MnNb has been investigated. Data on the load-flexibilty plot after impact test at various temperatures show that the steel either controlled-rolled or normalized offers higher resistance to tearing. The fracture occurred below the ductilebrittle transition temperature is by cleavage with dimpled rupture. The controlledrolled steel has a mixed α-grain structure which consists of equiaxial α-grains and "cold-worked" elongated grains with higher dislocation density, while the normalized steel has finer equiaxial α-grains with cell substructure of dislocation, of which the effective size of a-grain may be reduced. This microstructure of normalized steel makes the improved low-temperature impact property possible.
Received:  18 April 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I4/88

1 沈如璋;沈彼德;林有祚;王家禄;向德渊;叶崇发;李述创;栾凤英,钢铁,16(1981) ,№ 8,26.
2 Heslop, J.; Petch, N. J., Philos. Mag., 3 (1958) , 1128.
3 Tanaka, T., Int. Met. Rev., 26 (1981) , 185.z
No related articles found!
No Suggested Reading articles found!