Abstract The cleavage fracture stress of the dual phase steels has been evaluated with slow-bend test of blunt V-notched specimens. Their crack propagation path and fracture mode were indicated by the observations of the fracture morphology, the mieroeraek initiation and propagation of fracture surfaces under the cleavage temperature and the mierostrueture. According to the measurements of the cleavage fracture stress and the crack unit, the effective surface energy of the dual phase steels was also calculated by Griffith's equation. It was proposed that the cleavage fracture of the dual phase steels seems to be controlled by stress propagation and its regressive equation may be σ_f =0.33+19.33c~(-1/2) kgf/mm~2. Thus, the cleavage fracture stress may be increased by reducing the grain size of ferrite and martensite islands and by increasing the amount of evenly distributed lath martensite in the islands.
|
|
Received: 18 April 1983
|
1 马鸣图;吴宝榕,国外金属材料,(1981) ,№ 6,1. 2 Balliger, N. K.; Gladman, T., Met. Sci., 15 (1981) , 95. 3 Owen, W. S., Met. Technol., 7 (1980) , 1. 4 Davies, R. G.; Magee, C. L., Structure and Properties of Dual Phase Steel, Eds. Kot, R. A.; Morris, J. W., Jr., TMS/AIME, New York, 1979, p. 1-19. 5 Gerbase, J.; Embury, J. D.; Hobbs, R. M., ibid., p.118. 6 Becket, J.; Hornbogen, E.; Stratrnan, P., Z. Metallk., 71 (1980) , 27. 7 铃本驍一;荒木健治,金属,48(1978) ,№ 4,37. 8 Knott, J. F., Fundamentals of Fracture Mechanics, London, Butterworths, 1973, p. 176. 9 马鸣图;汪德根;吴宝榕,理化检验,A物理,18(1982) ,5,2. 10 Knott, J. F., Fracture, 1977, Vol.1, ICF4, Waterloo, Canada, June 1977, p.62. 11 Curry, D. A.; Knott, J. F., Met. Sci., 12 (1978) , 511. 12 Irwin. G. R., J. Appl. Mech., 29 (1962) . 651. 13 柳祖恩;蔡其巩,上海金属,(1982) ,№ 4,60.f |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|