PrPd_5——A NEW INTERMETALLIC COMPOUND
by CHEN Nianyi; XU Hua; ZHU Jianzhong; YANG Chuanzhen (Shanghai Institute of Metallurgy; Academia Sinica)
Cite this article: 

by CHEN Nianyi; XU Hua; ZHU Jianzhong; YANG Chuanzhen (Shanghai Institute of Metallurgy; Academia Sinica). PrPd_5——A NEW INTERMETALLIC COMPOUND. Acta Metall Sin, 1983, 19(3): 91-92.

Download:  PDF(137KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new intermetallic compound PrPd_5 was synthesized from individual pure metals. Its lattice parameters in comparison with MoAl_5 of well-known WAl_5-type structure are:a c c/aPrPd_5 4.97 8.996 1.81MoAl_5 4.89 8.80 1.80
Received:  18 March 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I3/91

1 Harris, I. R.; Raynor, G. V., J. Less-Common Met., 9 (1965) , 263.
2 Palenzona, A.; Iandelli, A., J. Less-Common Met., 34(1974) , 121.
3 陈念贻;徐桦;宁远涛,分子科学学报,1(1981) ,2,115.
No related articles found!
No Suggested Reading articles found!