| X-RAY LINE PROFILE ANALYSIS FOR MICRO-DISTORTION AND MOSAIC SIZE——AN APPROXIMATELY FUNCTIONAL GRAPHIC METHOD AND ATLAS OF WORKING GRAPH |
| by MENU Qing'en; ZHANG Zichang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
by MENU Qing'en; ZHANG Zichang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). X-RAY LINE PROFILE ANALYSIS FOR MICRO-DISTORTION AND MOSAIC SIZE——AN APPROXIMATELY FUNCTIONAL GRAPHIC METHOD AND ATLAS OF WORKING GRAPH. Acta Metall Sin, 1983, 19(3): 93-100.
|
|
|
Abstract An approximately functional graphic method and formulae for X-ray line frofile analysis of micro-distortion and mosaic structure were developed and a complete set of geometric broadening correction curves graph for this purpose was prepared.Considering the X-ray diffraction line pairs mostly selected in working on martensite and austenite materials and Ni-base alloys, based on the 5 radiations widely used in the laboratories, 35 kinds of separating m, n curves were plotted.
|
|
Received: 18 March 1983
|
1 Rachinger, W. A., Instrum. J. Sci., 25 (1948) , 254. 2 Gazzara, C. P.; Stiglich, J. J. Jr.; Meyer, F. P.; Hansen, A. M., Advances in X-Ray Analysis, Vol. 12, Plenum Press, New York, 1969, p. 257. 3 #12 4 许守廉,X射线金属学实验指导书,机械工业出版社,1966. 5 徐安达;张孝文,清华大学学报,11(1964) ,№ 4,21. 6 Klug, H. P.; Alexander, L. E., X-Ray Diffraction Procedures for Polycrystalline and Amorphous Materials, 2nd ed., Wiley, New York, 1974, p. 618. 7 Hall, W. H., Proc. Phys. Soc., (London), 62A (1949) , 741. 8 Hall, W. H., J. Inst. Met, 75 (1949) , 1127. 9 #12 10 #1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|