| STRESS EFFECT ON DOMAIN STRUCTURE OF GRAIN ORIENTED 3%Si-Fe Ⅱ. Compression Effect on Domain Structures |
| By LUO Yang; WANG Zhenqin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
By LUO Yang; WANG Zhenqin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). STRESS EFFECT ON DOMAIN STRUCTURE OF GRAIN ORIENTED 3%Si-Fe Ⅱ. Compression Effect on Domain Structures. Acta Metall Sin, 1983, 19(3): 23-146.
|
|
|
Abstract The compression effect on domain structure of grain oriented 3%Si-Fe was studied. As well known that if a compression is applied along rolling direction, then the domain magnetized along [001] would be energetically unfavourable. In that case the transverse domains magnetized along [100] or [010] are energetically favourable. So the latter would grow by the wall moving of the nuclei of transverse domains and become the main domain structure. As for the former main domain structure, then it would be degenerated into supplementary. Such stripe like pattern, which is parallel to [110], is so called transverse stripe pattern. With further increase of compression, these transverse stripe pattern would be broken into two groups of differently aligned tilting domain fragments, gradually. There are some correlations between the alignment of these tilting domain fragments and the crystallographic orientations. These two groups of tilting domain fragments intertwine with each other in rows and they are looked ike "λ". The higher the compression, the greater the volume fraction of "λ" domains. The row width and the space of domain fragment itself are also reduced with increase of compression. The cause of formation of such domains is discussed in the light of energy consideration. A model of "λ" domain structure is proposed in the present work.ě
|
|
Received: 18 March 1983
|
1 Moses, A. J.; Davies, D., IEEE Trans. Magn. MAG-16, (1980) , 454. 2 Swift, W. M., AIP Conf. Proc., (1975) , No. 29, 568. 3 罗阳;王振琴,金属学报,19(1983) ,A125. 4 Paxton, W. S.; Nilan, T. G., J. Appl. Phys., 26 (1955) , 994. 5 Goodenough, J. B., Phys. Rev., 102 (1956) , 356. 6 #12 7 Kittel, C., Rev. Mod. Phys., 21 (1949) , 541. 8 #12 9 Swift, W. M.; Wolfe, G. F., IEEE Trans. Magn., MAG-10 (1974) , 196. 10 McCurrie, R. A.; Martin, P. J.; Ashurst, S. J., J. Mater. Sci. 10 (1975) , 1788. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|