| OBSERVATION ON FATIGUE CRACK PROPAGATION OF PEARLITIC STRUCTURE |
| HU Zhizhong; ZHANG Pingsheng (Xi'an Jiaotong University) |
|
Cite this article:
HU Zhizhong; ZHANG Pingsheng (Xi'an Jiaotong University). OBSERVATION ON FATIGUE CRACK PROPAGATION OF PEARLITIC STRUCTURE. Acta Metall Sin, 1983, 19(2): 66-155.
|
|
|
Abstract Observations were demonstrated of 3 different types of the fatigue crack propagation of pearlitic structure: type A——the crack intersects the multiple ferrites and cementites simultaneously; type B——the crack cuts the ferrite and cementite one after another and type C——the crack propagates only through ferrite plate or along interface of ferrite and cementite. The fractographic examination indicated that the 3 fracture types in the process of fatigue crack propagation appear as different feature and proportion. In the slow stage of the fatigue crack propagation, it is the type A with partly type C or B; in the stable stage, mainly type A and B as well as marked fatigue striation; while in fast speed stage, the cleavage or dimple with partly striation predominantly.
|
|
Received: 18 February 1983
|
1 Miller, L. E.; Smieh, G. C., J. Iron Steel Inst,, 228 (1970) , 998. 2 Gurland, J., Acta Metall., 20 (1972) , 735. 3 Rosenfield, A. R.; Haha, G. T.; Embury, J. D., Metall. Trans., 3 (1972) , 2797. 4 Porter, D. A.; Easterling, K. E.; Smith, G. D. W., Acta Metall., 26 (1978) , 1405. 5 徐永波;刘民治;朱桂秋;于章,金属学报,4(1980) ,485. 6 增日千利;田中紘一;西岛敏,日本机械学会论文集,№.403,昭55-3,247. 7 胡志忠;郭大展;张平生;金雪贞,机械工程学报,1(1982) ,25. 8 周惠久,西安交通大学科学研究论文选集,(1978-80) ,274. 9 郭大展;胡志忠;安仁杰;王静宜,西安交通大学学报,6(1981) ,51.| |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|