Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (1): 31-142    DOI:
Current Issue | Archive | Adv Search |
A STUDY OF THE PREYIELDING MICROSTRAIN IN 3%Si-Fe ALLOY
ZHOU Bangxin
Cite this article: 

ZHOU Bangxin. A STUDY OF THE PREYIELDING MICROSTRAIN IN 3%Si-Fe ALLOY. Acta Metall Sin, 1983, 19(1): 31-142.

Download:  PDF(3048KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The preyielding microstrain process in polycrystalline 3%Si-Fe has been investigated with the method of displaying slip bands through electrolytic etching. Three different microstrain stages were found after analysis of the relations between the stress and the percentage of yielding grain and the average number of slip band per yielding grain. Plotted the starting stress at each microstrain stage against the reciprocal square root of grain diameter, three straight lines with different slop were obtained. Consideration of the Hall-Peteh relation, the Brown's microstrain theory and the upper yield point theory, the experimental results were discussed.
Received:  18 January 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I1/31

1 Suits, J. C.; Chalmers, B., Acta Metall., 9(1961) , 854.
2 Carrington, W. E.; McLean, D., ibid., 13(1965) , 493.
3 Worthington, P. J.; Smith, E., ibid., 12(1964) , 1277.
4 Tandon, K. N.; Tangri, K., Metall. Trans., 6A(1975) , 809.
5 周邦新,物理,9(1980) ,411.
6 Hook, R. E., Metall. Trans., 1(1970) , 85.
7 Merz, M. D.; Dahlgren, S. D., J. Appl. Phys., 46(1975) , 3235.
8 Miller, R. L., Metall. Trans., 3(1972) , 905.
9 Li, J. C. M.; Chou, Y. T., ibid., 1(1970) , 1145.
10 Hirth, J. P., ibid., 3(1972) , 3047.
11 Murr, L. E., ibid., 6A(1975) , 505.
12 Brown, N.; Lukens, K. F., Acta Metall., 9(1961) , 106.
13 Bilello, J. C.; Metzger, M., Trans. Metall. Soc. AIME., 245(1969) , 2279.
14 Cottrell,A.H.,晶体中的位错和范性流变,葛庭燧译,科学出版社,1960,p.153.
15 Johnston, W. G., J. Appl. Phys., 33(1962) , 2716.
16 Petch, N. J., Acta Metall., 12(1964) , 59.
17 Deep, G.; Plumtree, A., Metall. Trans., 6A(1975) , 359.
18 Hutchison, M. M.; Pascoe, R. T., Met. Sci., 6(1972) , 231.
19 Lloyd, D. J., ibid., 14(1980) , 193.
20 Douthwaite, R. M.; Evans, J. T., Acta Metall., 21(1973) , 525.
No related articles found!
No Suggested Reading articles found!