Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (1): 40-143    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF CYCLIC STRESS ON CREEP RUPTURE STRENGTH OF A CAST SUPERALLOY WITH HIGH Al AND Ti CONTENTS
BAI Yuankai(Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

BAI Yuankai(Institute of Metal Research; Academia Sinica; Shenyang). EFFECT OF CYCLIC STRESS ON CREEP RUPTURE STRENGTH OF A CAST SUPERALLOY WITH HIGH Al AND Ti CONTENTS. Acta Metall Sin, 1983, 19(1): 40-143.

Download:  PDF(1654KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of cyclic stress on the strength of creep rupture and recurrent creep rupture as well as low cycle fatigue of a cast nickel-base superalloy with high Al and Ti contents has been studied under different temperature and stress. It was found that the temperature is the main factor influenced upon the creepfatigue interaction. There are three temperature ranges leading to damage of creep, fatigue or combination of creep-fatigue individuaUy. The tested results were identified by some SEM fractographs.
Received:  18 January 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I1/40

1 横堀武夫,机械研究,28(1976) ,821.
2 Coffin, L. F., Fatigue at Eleveted Temperature, Ed. Carden, A. E., ASTM STP-520, 1972, p. 37.
3 Yeske, R. A.; Sommer, W.; Green, W. V., Symposium on Creep-Fatigue Interaction, Ed. Curran, R. M., ASME-MPC-3, 1976, p. 77.
4 Janson, J., Eng. Fract. Mech., 11(1979) , 397.
5 Grosskreutz, J. C., Metal Fatigue Damage, Ed. Manson, S. S., ASTM STP-465, 1970. p. 5; Wells, C. H.; Sullivan, C. P.; Gell, M., ibid., p. 61.
6 Viter, A.; Wibers, L. G., J. Met., 22(1970) , 5.
7 Coffin, L. F., Metall. Trans., 5(1974) , 1053.|
No related articles found!
No Suggested Reading articles found!