THE ETCH-PITS FEATURE OF BCC METALS AND ANALYTICAL TECHNIQUE FOR QUANTITATIVE DETERMINATION OF THEIR GRAIN ORIENTATION
Liao Qianchu; Wang Hongjun; Wang Yun; Lan Fenlan (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

Liao Qianchu; Wang Hongjun; Wang Yun; Lan Fenlan (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). THE ETCH-PITS FEATURE OF BCC METALS AND ANALYTICAL TECHNIQUE FOR QUANTITATIVE DETERMINATION OF THEIR GRAIN ORIENTATION. Acta Metall Sin, 1982, 18(6): 713-725.

Download:  PDF(2030KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

By means of metallographic microscope and SEM the correlation between the feature of etch-pits and the grain orientations in bcc metals has been investigated. The grain orientations were determined by ECP in SEM and illustrated in a unit stereograph triangle. A series of their relational expressions was deduced with aid of vector analysis and coordinate transformation method. Some tables and charts, on which the grain orientation can be rapidly consulted, have been constructed by collection of the theoretically computed data. The analyzed results of the grain orientations may be directly expressed in a unit stereograph triangle and also easily determined on the transformation matrix of the grain boundaries, because the shapes of etch-pits are described by a continuous function of azimuth angle (θ, φ). Certain metallurgical problems have been discussed by the application of this analytical technique.

Received:  18 June 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I6/713

1 Matsuda, S.; Okamura, Y., Trans. Jpn. Inst. Met., 11(1970) , 371. 2 小寺沢良一;志茂大冶郎,材料,26(1977) ,730. 3 罗阳;吕其春,金属学报,13(1973) ,194. 4 村田雅人;向井喜彦,日本金属学会志,44(1980) ,713. 5 Betz, E. T.; Prohaszka, J., Metallography, 7(1974) , 91.
No related articles found!
No Suggested Reading articles found!