Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (5): 581-653    DOI:
Current Issue | Archive | Adv Search |
THE MODIFICATION OF Si PHASE IN Al-Si EUTECTIC ALLOYS——Effect of Element Addition on Microstructures of Al-Si and Al-Si-Ge Eutectic Alloys
Zhang Qiyun; Liu Shuqi; Fan Xiaohong (Department of Chemistry; Beijing University)
Cite this article: 

Zhang Qiyun; Liu Shuqi; Fan Xiaohong (Department of Chemistry; Beijing University). THE MODIFICATION OF Si PHASE IN Al-Si EUTECTIC ALLOYS——Effect of Element Addition on Microstructures of Al-Si and Al-Si-Ge Eutectic Alloys. Acta Metall Sin, 1982, 18(5): 581-653.

Download:  PDF(2226KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of micro-amount element additions on the microstructures of Al-Ge and Al-Si-Ge eutectic alloys has been studied by means of metallographic method. For Al-Ge eutectics, no evidence was found of occurring any modification something like that exists in the Al-Si system. Some elements which belong to the ⅣB, ⅤB and ⅥB groups in the periodic table of elements seriously influence their microstructures and change the feather-like Al-Ge euteetic into block Ge crystals. In the other case, it appears to move the eutectic point to the Al-rich side when some alkaline, alkaline earth and rare earth elements were added in this eutectic. The modifiers Na, Sr, La effective in the Al-Si system were scanned about their effects on the Al-Si-Ge system. In this ease, eutectic Si exists in modified clusters form and gradually dwindle their size with increasing the Ge content, finally they disappeared at the Al-Ge side. According to comparison of the modification between the Al-Ge and Al-Si systems, it was considered that the modification of Al-Si eutectic was mainly decided by the effects of modifier atoms on the epitaxial orientation relationship or decreasing the disregistry between {110}_(Si) and {100}_(Al).
Received:  18 May 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I5/581

1 Day, M. G.; Hellawell, A., J. Inst. Met., 95(1967) , 377.
2 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 23.
3 #12
4#12
5 Pech, G. J.; Thesis, M. S., LBL 7300,(1977) , p. 6.
6 刘淑祺;孙国平;张启运,金属学报,18(1982) ,451.
7 Hellawell, A., Trans Metall. Soc. AIME, 239(1967) , 1049.
8 Day, M. G., J. Inst. Met., 98(1970) , 57.
9 朱培钺;陈熙琛;贾均;张宝书;刘贤功,未发表资料,1979.
10 Hellawell, A., Progress in Materials Science, Vol. 15, Part Ⅰ, Pergamon, London 1970, p. 47.
11 张启运;郑朝贵;韩万书,金属学报,17(1981) ,130
No related articles found!