Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (5): 586-591    DOI:
Current Issue | Archive | Adv Search |
AN AES STUDY OF ANODIC OXIDE FILM ON 1Cr18Ni9 STAINLESS STEEL
Lin Rongfu; Dai Daoxuan; Dong Shuzhong (Department of physics; Fudan University; Shanghai); Zou Huiliang; Luo Xinghua (Shanghai Institute of Measuring and Testing)
Cite this article: 

Lin Rongfu; Dai Daoxuan; Dong Shuzhong (Department of physics; Fudan University; Shanghai); Zou Huiliang; Luo Xinghua (Shanghai Institute of Measuring and Testing). AN AES STUDY OF ANODIC OXIDE FILM ON 1Cr18Ni9 STAINLESS STEEL. Acta Metall Sin, 1982, 18(5): 586-591.

Download:  PDF(507KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The AES has been used to study the composition of the anodic oxide film on 1Cr18Ni9 stainless steel. The film was formed in the transpassive region during the constant potential anodic polarization in H_2SO_4 and after a treatment with Na_2MoO_4. It has been found that the outer layer of the film contains a lot of Mo and the middle layer is rich in Cr. The concentration of oxygen in the rest of the layer up to the interface rapidly reduces to zero. The middle layer in the transpassive anodic oxide film which is rich in Cr is more wider and oxidized more complete than that in HNO_3 oxide film. By comparison with other oxide films, the possible mechanisms for passivation of transpassive anodic polarization are discussed.
Received:  18 May 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I5/586

1 Seo, M.; Sato, N.; Lumsden, J. B., Corros. Sci., 17(1977) , 209.
2 Yaniv, A. E.; Lumsden, J. B.; Staehle, R. W., J. Electrochem. Soc., 124(1977) , 490.
3 Cunha Belo, M. da; Rondot, B.; Pons, F.; Le Hericy, J.; Langeron, J. P., J. Electrochem. Soc., 124(1977) , 1317.
4 Olefjord, I., Corros. Sci., 15(1975) , 687.
5 Olefjord, I.; Fischmeister, H., ibid., 15(1975) , 697.
6 Castle, J. E.; Clayton, C. R., ibid, 17(1977) , 7.
7 Asami, K.; Hashimoto, K.; Shimodaira, S., ibid., 18(1978) , 151.
8 Lewis, G.; Chappell, M. J., ibid., 19(1979) , 73.
9 Hara, N.; Sugimoto, K., J. Electrochem. Soc., 126(1979) , 1328.
10 Seo, M.; Saito, R.; Saito, N., ibid., 127(1980) , 1909.
11 张永福;包伟国;江绍猷;吕国梁;林荣富;戴道宝;董树忠;黄国柱;徐克薰,金属学报,17(1981) ,529.
12 Klasson, M.; Hedman, J.; Bemdtsson, A.; Nilsson, R.; Nordling, C., Phys. Scr., 5(1972) , 93.
13 Chang, C. C., Characterization of Solid Surfaces, Es., P. F. Kane; G. B., Larrbee, Plenum Press, New York, 1974, p. 509.
14 Handbook of Auger Electron Spectroscopy, Es. L. E. Davis, et al., Physical Electronics Industries, Inc., Eden Prairie, 1976, p. 77, 83, 91 etc.
15 Lumsden, J. B.; Staehle, R. W., Am. Soc. Test. Mater., Spec. Tech. Publ., №. 596,(1976) .
16 Pourbaix M. Atlas of Electrochemical Equilibria in Aqueous Solutions, Pergamon Press, New York, 1966, p. 268, 311.Z