A STUDY ON HIGH TEMPERATURE TEMPER BRITTLENESS BY INTERNAL FRICTION MEASUREMENTS
Lei Tingquan Tang Zhixiou Su Mei (Harbin Institute of Technology) (Manuscript received 26 March; 1981; revised manuscript 18 October; 1981)
Cite this article: 

Lei Tingquan Tang Zhixiou Su Mei (Harbin Institute of Technology) (Manuscript received 26 March; 1981; revised manuscript 18 October; 1981). A STUDY ON HIGH TEMPERATURE TEMPER BRITTLENESS BY INTERNAL FRICTION MEASUREMENTS. Acta Metall Sin, 1982, 18(4): 485-524.

Download:  PDF(1092KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The impact toughness, low frequency internal friction and TEM examination were tested for steels 40Mn2, 40Mn2Mo and 30CrMnSiNi2. Experimental results indicate that the appearance of high temperature temper brittleness in these steels seems to be always accompanied by the decrease of Koster peak heights. The mechanism of this phenomenon may be explained as the result of an aging process of α-α-solid solution with precipitation of Fe_3C(N)particles causing pinning of dislocations and thereby decreasing the impact toughness.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/485

1 Woodfine, B.C., J. Iron Steel Inst., 173(1953) , 240.
2 Low, J.R., Fracture of Engineering Materials, ASM, 1964, p.127.
3 Olefjord, I., Int. Metall. Rev., 4(1978) , 149.
4 Restnaio, P.A.; McMahon, C.J., Jr., ASM Trans. Q., 60(1967) , 699.
5 Schulz, B.J.; McMahon, C.J., Jr., Am. Soc. Test. Mater. Spec. Tech. Publ.,499,(1971) , p. 104.
6 Ohtani, H.; Feng, H.C.; McMahon, C.J., Jr., Metall. Trans., 5(1974) , 516.
7 Jin Yu; McMahon, C.J., Jr., Metall. Trans., 11A(1980) , 277, 291.
8 曲哲;郭可信,金属学报,16(1980) ,371.
9 Wada, T.; Doane, D.V., Metall. Trans., 5(1974) , 231.
10#12
No related articles found!
No Suggested Reading articles found!