THE PHASE DIAGRAM OF SYSTEM Al-Si-Ge
Liu Shuqi Sun Guoping Zhang Qiyun (Department of Chemistry; Beijing University) (Manuscript received 2 February; 1981; revised manuscript 13 January; 1982)
Cite this article: 

Liu Shuqi Sun Guoping Zhang Qiyun (Department of Chemistry; Beijing University) (Manuscript received 2 February; 1981; revised manuscript 13 January; 1982). THE PHASE DIAGRAM OF SYSTEM Al-Si-Ge. Acta Metall Sin, 1982, 18(4): 451-523.

Download:  PDF(969KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

A polythermal phase diagram study has been made of the Al-rich part in the AI-Si-Ge system by the methods of thermal analysis and metallography. The system belongs in a eutectic type with continuous transition from one binary side to the another. The temperatures of the eutectic line gradually decrease from 577℃ on the Al-Si side to 423℃ on the Al-Ge side. The orthogonally projected eutectic line is slightly convex to the Al-corner from the connected line of two eutectics on the both binary sides. No evidence was found about any new compound and phase in the system.

Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/451

1 Block, H.H., U.S. Pat., 2 508 008,(1950) . 2 Werner, W.J., U.S. Pat., 3 791 820,(1974) . 3 桑野明良,日本公开特许公报,52-33860,(1977) . 4 Hansen, M., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 133. 5 Hansen, M. ibid., p. 97. 6 Hansen, M., ibid., p. 774.
No related articles found!
No Suggested Reading articles found!