| ON THE OXYGEN PARTIAL PRESSURE AND ACTIVITY OF FeTiO_3-MgTiO_3 SOLID-SOLUTION SYSTEM |
| LI Guoxun; Cao Rongjiang (General Research Institute of Nonferrous Metals; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
LI Guoxun; Cao Rongjiang (General Research Institute of Nonferrous Metals; Ministry of Metallurgical Industry; Beijing). ON THE OXYGEN PARTIAL PRESSURE AND ACTIVITY OF FeTiO_3-MgTiO_3 SOLID-SOLUTION SYSTEM. Acta Metall Sin, 1982, 18(3): 371-377.
|
|
|
Abstract The oxygen partial pressure and activity of FeTiO_3-MgTiO_3 solid-solution system were studied by means of oxygen concentration cell with the solid electrolyte. Taken Fe/FeO as reference electrode, the oxygen partial pressure was measured, and standard free enthalpy of formation of non-stoichiometric FeO (w/istite) was obtained as ΔG_(FeO)~0=-259030+60.25T (J·mol~(-1)). Furthermore, the oxygen partial pressure and wustite activity of the various compositions of the solid-solution system were measured at the temperature range of 900—1200℃. The results show that both values increase with the increase of temperature. The standard free enthalpy of formation of complex oxide FeTiO_3, ΔG_(FeTiO_3)~0=-40470+19.75T (J·mol~(-1)) and the activity-composition relation of this solid-solution series were obtained.
|
|
Received: 18 March 1982
|
1 Johnson, R. E.; Woermann, E.; Muan, A., Am. J. Sci., 271 (1971) , 278. 2 Seetharaman, S.; Abraham, K. P., Indian J. Technol., 6 (1968) , No. 4, 123. 3 Engcll, H.-J., Z. Phys. Chem. Neue Folge, 35 (1962) , 192. 4 北京钢铁学院编,冶金过程物理化学研究方法,1975,下册,p.475. 5 Reed, Thomas, B., Free Energy of Formation of Binary Compounds, MIT Press, Cambridge, Mass, 1971. 6 Taylor, R. W.; Schmalzricd, H., J. Phys. Chem., 68 (1964) , 2444. 7 Richardson, F. D.; Jefes, J. H. E., J. Iron Steel Inst., 163 (1949) , 397. 8 小野勝敏,森山徐一郎,日本鉱业会誌,89(1973) ,No.5,313. 9 Haggerty, S. E.; Lindsley, D. H., Carnegie Inst. Washington, Yearbook, 1968-1969. Pub. 1970, p.247-9. 10 Kubaschcwski, O., High Temp. High Pressures,4 (1972) , No. 1,1. 11 Richardson, F. D.; Jeffes, J. H. E.; Withers, G., J. Iron Steel Inst., 166 (1950) , 213. 12 Grey, E.; Reid, A. E.; Jones, D. G., Trans. Inst. Min. Metall., Sect. C, 83 (1974) , No. 811, C 105.X |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|