METALLURGICAL PROCESS SIMULATION
Xu Zhihong; Wang Daguang; Xia Yongnian; Che Xiuzhen; Wang Leshan; Ai Jing (Institute of Chemical Metallurgy;Academia Sinica; Beijing)
Cite this article: 

Xu Zhihong; Wang Daguang; Xia Yongnian; Che Xiuzhen; Wang Leshan; Ai Jing (Institute of Chemical Metallurgy;Academia Sinica; Beijing). METALLURGICAL PROCESS SIMULATION. Acta Metall Sin, 1982, 18(3): 361-370.

Download:  PDF(747KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An effort was made in the fields of setting up the metallurgical process modules and the process system simulation programs which include: general principles and examples of metallurgical process simulation; the dynamic simulation of chemical metallurgical processes and inorganic thermochemical data base and its applications in metallurgical process simulation.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/361

1 Peterson, J. N.; Chen, C. C.; Evans, L. B., Chem. Eng., (1978) , No. 6, 5, 145; No. 7, 3, 69; No. 7, 31, 79; (1979) , No. 5, 21, 167.
2 Izurieta, H.; Edward, L. L, J. Met., 32 (1980) , No. 12, 23.
3 Weeks, R., Mathematical Process Models in Iron and Steelmaking, Proc. of the Conferences Organized by the Iron and Steel Institute, Ed. Van Langen, J. M. et al., Metals Society, London, 1973, p. 103.
4 Middleton, J. R.; Rolls, R., ibid., p. 117.
5 Greenfield, A. A., ibid., p. 125.
6 Asai, S.; Muchi, I., ibid., p. 134.
7 Surguchov, G. D., Met. Mater., (1978) , No, 7, 38.
8 马朴京,钢铁,(1979) ,No.3,38.
9 Ward, R. G., An Introduction to the Physical Chemistry of Iron and Steelmaking, 1962, Edward Arnold Ltd., p. 102.
10 Barin, T; Knacke, O., Thermochemical Properties of Inorganic Substances, Berlin, Springer, 1973.3
No related articles found!
No Suggested Reading articles found!