Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (3): 350-394    DOI:
Current Issue | Archive | Adv Search |
ON THE DISLOCATION SLIP MECHANISM OF THE MARTENSITIC TRANSFORMATION OF STEELS
Lin Baojun (Nei Monggol Institute of Metallic Materials; Baotou; Nei Monggol Autonomous Region)
Cite this article: 

Lin Baojun (Nei Monggol Institute of Metallic Materials; Baotou; Nei Monggol Autonomous Region). ON THE DISLOCATION SLIP MECHANISM OF THE MARTENSITIC TRANSFORMATION OF STEELS. Acta Metall Sin, 1982, 18(3): 350-394.

Download:  PDF(2480KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  With the aid of TEM observation on the martensite transformation of three steels, the relative position changes between atoms caused by the dislocation slip during fcc→bcc (or bet)lattice variation are mainly carried through shears in combination with different slip systems along<112>_f/{111}_f in the distorted fee lattice. Two types of these changes are: (1) the atom displacement of main shear only along one slip system of (1/m)<112>_f/{111}_f and (2)M=(1/n)[<112>_(f1)/{111}_(f1)+<112>_(f2)/{111}_(f2)] complex displacement obtained by all dislocations operated in different {111}_f conjugate sIip plane (n>6). Thus, an atom displacement mechanism of which the austenite transforms into martensite through conjugate complex slips of partial dislocation during quenching has been proposed. Based upon this mechanism, the crystalline geometry explanation may be undoubtedly made on the orientation correlation between matensite and austenite matrix, as well as the martensite habit planes and some special phenomena in quenched martensite.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/350

1 西山善次,变態,(基本篇),丸善,东京,1972,p.16,282.
2 Fujita, F. E., Metall. Trans., 8A (1977) , 1727.
3 Narasimha Rao, B. V., Metall. Trans., 10A (1979) , 645.
4 Olson, G. B.; Cohen, M., Metall.Trans., 7A (1976) , 1905.
5 Narasimha Rao, B. V.; Thomas, G., 待发表.
6 Oshima, R.; Azuma, H.; Fujita, F. E., Scr. MetaIl, 10 (1976) , 1011.
7 Foos, M.; Frantz, C.; Gantois, M., Scr. Metall., 12 (1978) , 795.
8 Hausch, G., J. Phys. Soc. Jpn., 37 (1974) , 819, 824.
9 郭可信,林保军,物理学报,27(1978) ,729.
10 郭可信,林保军,物理学报,29(1980) ,494.
11 Howie, A.; Whelan, M. J., Proc R. Soc., London A267 (1962) , 206.
12 Howell, P. R.; Jones, A. R., J. Mater. Sci., 13 (1978) , 1803.
13 Whelan, M. J.; Hirsch, P. B., Philos. Mag., 2 (1957) , 1211, 1303.
14 Cornelis, I.; Oshima, R.; Tong, H. C.; Wayman, C. M., Scr. Metall., 8 (1974) , 133.
15 徐祖耀,马氏体相变与马氏体,科学出版社,北京,1980,p.99,376,403.
16 Shimizu, S.; Nishiyama, Z., Phase Transformation and Related Phenomenal in Steel, ASM, 1971, p. 1055.
17 Sarma, D. S.; Whiteman, J. A.; Woodhead, J. H., Met. Sci., 10 (1976) , 391.
18 Brook, R.; Entwisle, A. R,, J. Iron Steel Inst., 203 (1965) ,905.
19 Thomas, G., Metall. Trans., 2 (1971) , 2373.
20 Shimizu, K.; Oka, M.; Wayman, C. M., Acta Metall., 18 (1970) , 1005.d