AN X-RAY DIFFRACTION TOPOGRAPHIC METHOD AND ITS APPLICATION TO FRACTURE PROBLEM OF METAL
An Zhengzhi; Ha Kuanfu (Jilin University; Changchuan)
Cite this article: 

An Zhengzhi; Ha Kuanfu (Jilin University; Changchuan). AN X-RAY DIFFRACTION TOPOGRAPHIC METHOD AND ITS APPLICATION TO FRACTURE PROBLEM OF METAL. Acta Metall Sin, 1982, 18(3): 286-292.

Download:  PDF(3225KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new X-ray diffraction topographic method was developed and used to study the fracture morphology and process in three point bending test of Mo single crystals. It was shown that not only the different regions similar to ones of optical fractograph, namely, unstable and stable extension regions, as well as triangle region formed by tearing, but also the different orientated subgrains, subgrains' rupture and their stress states may be revealed from the X-ray diffraction pattern. By the fracture process investigation, the subgrain rotation, the lattice bending and the spreading of plastic zone were found in front of the precracks.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/286

No related articles found!
No Suggested Reading articles found!