| A NOTE ON RELATIONSHIP BETWEEN MARTENSITE MORPHOLOGY AND SHAPE MEMORY EFFECT OF A Cu-Al-Ni ALLOY |
| Tan Shusong; Huang Jianchao; Sun Xiaohua; Tan Xuecheng (Central-South Institute of Mining and Metallurgy; Changsha) |
|
Cite this article:
Tan Shusong; Huang Jianchao; Sun Xiaohua; Tan Xuecheng (Central-South Institute of Mining and Metallurgy; Changsha). A NOTE ON RELATIONSHIP BETWEEN MARTENSITE MORPHOLOGY AND SHAPE MEMORY EFFECT OF A Cu-Al-Ni ALLOY. Acta Metall Sin, 1982, 18(3): 281-391.
|
|
|
Abstract A direct observation under different temperature and stress is reported of the martensite morphology variation vs the longitudinal change in a Cu-Al-Ni alloy specimen. The results indicate that its pseudo-elasticity and shape memory effect are closely related to the variation of martensite morphology.
|
|
Received: 18 March 1982
|
1 Krishnan, R. V.; Delaey, L.; Tas, H.; Warlimont, H., J. Mater. Sci., 9 (1974) , 1536. 2 Shimizu, K.; Otsuka, K., Shape Memory Effects, Ed. Perkins J., Planum Press, New York, 1975, p. 59. |