FUZZY SYMMETRIC GROUP AND SHORT-RANGE ORDER IN THE STRUCTURE OF AMORPHOUS SOLIDS
Zheng Zhaobo (University of Science and Technology of China; recently engaged in advanced studies at Department of Physics; University of Louisville; Kentucky; U. S. A.; when the reseaech was carried out)
Cite this article: 

Zheng Zhaobo (University of Science and Technology of China; recently engaged in advanced studies at Department of Physics; University of Louisville; Kentucky; U. S. A.; when the reseaech was carried out). FUZZY SYMMETRIC GROUP AND SHORT-RANGE ORDER IN THE STRUCTURE OF AMORPHOUS SOLIDS. Acta Metall Sin, 1981, 17(6): 643-651.

Download:  PDF(748KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A concept, Fuzzy symmetric group, is introduced and subsequently applied to the description of short-range order in the structure of amorphous solids.
Received:  18 June 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I6/643

[1] Finney, J. L., Nature, 266 (1977) , 309.
[2] 干福熹,科学通报,2(1963) ,18.
[3] 干福熹,硅酸盐学报,7(1979) ,150.
[4] 干福熹,中国科学,(1974) ,№.4,351.
[5] 早稻田嘉夫,固体物理,12(1977) ,181.
[6] Bernal, J. D., Nature, 183 (1959) , 141.
[7] Kanfmann, A., Introduction to the Theory of Fuzzy Subsets, Vol. 1, Academic Press, New York, 1975, p. 3.
[8] Connell, G. A. N. and Lucovsky, G., Non-Cryst. Solids, 31 (1978) , 123.`
No related articles found!
No Suggested Reading articles found!